TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics’ Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in color, and combine exceptional mechanical, thermal, and electrical properties. The addition of glass fiber reinforcement in the 2000 series, coupled with Ensinger’s proprietary extrusion techniques, provides the TECAPEI™ with both greater tensile
- Excellent mechanical strength
TECAPEI™ exhibits high tensile strength at room temperature and retains a significant portion of this strength at elevated temperatures.
Glass fibers further increase high-temperature strength. - Outstanding heat resistance
TECAPEI™ retains its physical properties at elevated temperatures. - Exceptional resistance to environmental forces
Environmental characteristics of TECAPEI™ include it’s stress resistance. - Inherent flame resistance with low smoke evolution
Tested internally to UL 94 V-0. - High mechanical strength
- High dielectric strength
- Low dissipation factor over a wide range of frequencies
- Excellent machinability and finishing characteristics
TECAPEI has many applications in medical, electronic/electrical, microwave, automotive, and aircraft industries.
Properties | Condition | Value | Test Method | Comment | ||
---|---|---|---|---|---|---|
Mechanical | Modulus of elasticity (tensile test) | @ 73°F | 430,000 | psi | ASTM D 638 | |
Tensile strength at break | @ 73°F | 16,500 | psi | ASTM D 638 | ||
Elongation at yeild | @ 73°F | 7-8 | % | ASTM D 638 | ||
Elongation at break | @ 73°F | 40 | % | ASTM D 638 | ||
Flexural Strength | @ 73°F | 22,000 | psi | ASTM D 790 | ||
Modulus of Elasticity (flexural test) | @ 73°F | 480,000 | psi | ASTM D 790 | ||
Compression strength | @ 10% strain | 21,900 | psi | ASTM D 695 | ||
Compression strength | @ 1% strain | 2,200 | psi | ASTM D 695 | ||
Notched impact strength (Izod) | @ 73°F | 0.60 | ft-lbs/in | ASTM D 256 | ||
Rockwell hardness | M Scale | 111 | % | ASTM D 785 | ||
Thermal | Vicat softening point | 426 | °F | ASTM D1525 1) | 1) Injection molded data | |
Deflection temperature | @ 246 psi | 394 | °F | ASTM D 648 1) | ||
Deflection temperature | @ 66 psi | 410 | °F | ASTM D 648 1) | ||
Thermal expansion (CLTE) | 3.1*10-5 | in/in/°F | ASTM D 696 1) | |||
Thermal conductivity | 1.5 | BTU-in/hr-ft2-°F | ASTM D 2214 1) | |||
Electrical | Volume resistivity | 1/16 | 1.0×1017 | Ω*cm | ASTM D 257 1) | |
Dielectric strength | In Oil | 709 | V/mil | ASTM D 149 1) | ||
Dielectric strength | In Air | 830 | V/mil | ASTM D 149 1) | ||
Dissipation factor | 1 kHz, 50% RH, 73 °F | 0.0013 | ASTM D 150 1) | |||
Dielectric constant | 1 kHz, 50% RH | 3.15 | ASTM D 150 1) | |||
Other | Moisture absorption | @ 24 hrs, 73°F | 0.25 | % | ASTM D 570 1) | 2) Injection molded data (0.75 mm thickness) |
Moisture absorption | @ saturation, 73°F | 1.25 | % | ASTM D 570 1) | ||
Flammability (UL94) | V-0 | 2) |